当前位置:首页-新闻中心新闻中心

不锈钢螺旋风管出现浸蚀时一定要留意这些情况

发布人:http://www.sftfgd.com   发布时间:2022-06-01 19:24:00

不锈钢螺旋风管出现浸蚀时请留意

Please pay attention to corrosion of stainless steel spiral air duct

常耐用?当它表层出现这些现象时请注意了。

Constant use? Please pay attention when these phenomena appear on its surface.

现象一:不锈钢螺旋风管的部分出现生锈。

Phenomenon 1: part of the stainless steel spiral air duct is rusted.

现象一:不锈钢螺旋风管表层出现一些擦毛、脏物等。

Phenomenon 1: there are some scratches and dirt on the surface of stainless steel spiral air duct.

现象三:在焊接表层,其色调是呈灰黑色的,或是是有黄点或斑点。

Phenomenon 3: on the welding surface, the color is grayish black, or there are yellow spots or spots.

这三种状况,一旦出现这些现象得话,不锈钢螺旋风管厂家告诉你它的耐腐蚀工作能力、使用寿命正在减少。

In these three cases, once these phenomena occur, the manufacturer of stainless steel spiral air duct will tell you that its corrosion resistance and service life are decreasing.

什么缘故导致浸蚀呢?

What causes erosion?

1、不锈钢螺旋风管所应用的板才,其开料或生产加工具体方法不善。

1. For the plate used in the stainless steel spiral air duct, the specific methods of cutting or production and processing are not good.

2、不锈钢螺旋风管在生产加工生产制造全过程中,就出现了浸蚀状况,但并没有立即开展解决。

2. The stainless steel spiral air duct was corroded in the whole process of manufacturing, but it was not solved immediately.

3、不锈钢螺旋风管的焊接工艺没有挑选恰当,也就是焊接工艺不善。

3. The welding process of stainless steel spiral air duct is not properly selected, that is, the welding process is poor.

4、不锈钢螺旋风管电焊焊接好之后,没有立即开展清理和。

4. The stainless steel spiral air duct was not cleaned and removed immediately after electric welding.

本文的精彩内容由济南风管加工厂提供知识提供,本网站还有很多的精彩内容,更多的内容您可以点击进入:http://www.sftfgd.com我们有专门的客服为您解答问题

The wonderful contents of this article are provided by Jinan air duct processing factory. There are many wonderful contents on this website. You can click to enter more contents: http://www.sftfgd.com We have special customer service to answer your questions


上一篇:通风管道制作前怎么挑选适宜的原材料?
下一篇:避免通风管道腐蚀的条件具体有哪些呢